General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.3 g/cm³ Show Supplier Material materials with Density of 1.3 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Water absorption | 0.45 % Show Supplier Material materials with Water absorption of 0.45 % | dry | Sim. to ISO 62 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 250 °C | 75 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 75 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |