General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 66 % Show Supplier Material materials with Bio-based content of 66 % | dry | ASTM D6866-12 Method B |
Density | 1.08 g/cm³ Show Supplier Material materials with Density of 1.08 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 1.3 GPa Show Supplier Material materials with Elastic modulus of 1.3 GPa | conditioned | ISO 527-1/-2 | ||
2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | dry | ISO 527-1/-2 | |||
Elongation | 45 % Show Supplier Material materials with Elongation of 45 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongation of 50 % | conditioned | ISO 527-1/-2 | |||
Flexural modulus | 1.3 GPa Show Supplier Material materials with Flexural modulus of 1.3 GPa | conditioned | ISO 178 | ||
2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | dry | ISO 178 | |||
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | ||
95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | |||
Hardness, Shore D | 78 [-] Show Supplier Material materials with Hardness, Shore D of 78 [-] | dry | ISO 868 | 15s | |
Impact strength, Charpy notched | -30 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | conditioned | ISO 179/1eA | ||
Tensile strength | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | conditioned | ISO 527-1/-2 | ||
65 MPa Show Supplier Material materials with Tensile strength of 65 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 76 °C Show Supplier Material materials with Heat deflection temperature of 76 °C | dry | ISO 75-1/-2 | 2 MPa | |
165 °C Show Supplier Material materials with Heat deflection temperature of 165 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | conditioned | IEC 60112 |
Dielectric strength | 30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | conditioned | IEC 60243-1 |
34 kV/mm Show Supplier Material materials with Dielectric strength of 34 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | conditioned | IEC 62631-3-1 |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |