General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 0.77 g/cm³ Show Supplier Material materials with Density of 0.77 g/cm³ | dry | ISO 60 |
1.24 g/cm³ Show Supplier Material materials with Density of 1.24 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Water absorption | 0.6 % Show Supplier Material materials with Water absorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 0.28 GPa Show Supplier Material materials with Elastic modulus of 0.28 GPa | dry | ISO 527-1/-2 | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | ||
Hardness, Shore D | 59 [-] Show Supplier Material materials with Hardness, Shore D of 59 [-] | dry | ISO 868 | 3s | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
Tear strength | 152 kN/m Show Supplier Material materials with Tear strength of 152 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 36 MPa Show Supplier Material materials with Tensile strength of 36 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1.85e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.85e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.85e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.85e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | -60 °C Show Supplier Material materials with Glass transition temperature of -60 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 115 °C Show Supplier Material materials with Heat deflection temperature of 115 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 212 °C Show Supplier Material materials with Melting point of 212 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Vicat softening temperature | 125 °C Show Supplier Material materials with Vicat softening temperature of 125 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 3.4 [-] Show Supplier Material materials with Dielectric constant of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 22 kV/mm Show Supplier Material materials with Dielectric strength of 22 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 110 [-] Show Supplier Material materials with Dissipation factor of 110 [-] | dry | IEC 62631-2-1 | 100Hz |
340 [-] Show Supplier Material materials with Dissipation factor of 340 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 28.0 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 28.0 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.75 % Show Supplier Material materials with Shrinkage of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Shrinkage of 2 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Snowboard Binding Straps, Optical Fiber loose buffer tubes | |
Certifications | Food Contact, Yellow Card Available |