General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.43 g/cm³ Show Supplier Material materials with Density of 1.43 g/cm³ | dry | ISO 1183 | |
Limiting oxygen index | 29.0 % Show Supplier Material materials with Limiting oxygen index of 29.0 % | dry | ISO 4589-1/-2 | |
Moisture absorption | 2.35 % Show Supplier Material materials with Moisture absorption of 2.35 % | dry | Sim. to ISO 62 | |
Water absorption | 2.4 % Show Supplier Material materials with Water absorption of 2.4 % | dry | ISO 62 | at 23°C after 24h |
8.6 % Show Supplier Material materials with Water absorption of 8.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.4 GPa Show Supplier Material materials with Elastic modulus of 3.4 GPa | dry | ISO 527-1/-2 | |
Elongation | 7 % Show Supplier Material materials with Elongation of 7 % | dry | ISO 527-1/-2 | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | dry | ISO 178 | |
Flexural yield strength | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | dry | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 225 V Show Supplier Material materials with Comparative tracking index of 225 V | dry | IEC 60112 | |
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.1 [-] Show Supplier Material materials with Dielectric constant of 4.1 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Dielectric constant of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 50 [-] Show Supplier Material materials with Dissipation factor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Dissipation factor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
800 [-] Show Supplier Material materials with Dissipation factor of 800 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
2800 [-] Show Supplier Material materials with Dissipation factor of 2800 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1140 g/cm³ Show Supplier Material materials with Density of melt of 1140 g/cm³ | dry | - | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal | |
Thermal conductivity of melt | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |