General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.38 g/cm³ Show Supplier Material materials with Density of 1.38 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 6.5 GPa Show Supplier Material materials with Elastic modulus of 6.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.8 % Show Supplier Material materials with Elongation of 2.8 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA |
Tensile strength | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure |
---|---|---|---|---|
Heat deflection temperature | 183 °C Show Supplier Material materials with Heat deflection temperature of 183 °C | dry | ISO 75-1/-2 | 2 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |