General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Water absorption | 0.55 % Show Supplier Material materials with Water absorption of 0.55 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 1 GPa Show Supplier Material materials with Elastic modulus of 1 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | dry | ISO 527-1/-2 | |
Flexural modulus | 0.9 GPa Show Supplier Material materials with Flexural modulus of 0.9 GPa | dry | ISO 178 | |
Hardness, Shore D | 56.0 [-] Show Supplier Material materials with Hardness, Shore D of 56.0 [-] | dry | ISO 868 | 15s |
Tensile strength | 18 MPa Show Supplier Material materials with Tensile strength of 18 MPa | dry | ISO 527-1/-2 |
Thermal
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt mass-flow rate | 230 °C | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Chair Carriers, Seat Suspension/Fabrics | |
Fillers | Glass Fiber |