General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.3 g/cm³ Show Supplier Material materials with Density of 1.3 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Water absorption | 0.45 % Show Supplier Material materials with Water absorption of 0.45 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 2.7 GPa Show Supplier Material materials with Elastic modulus of 2.7 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | dry | ISO 178 | |
Flexural yield strength | 89 MPa Show Supplier Material materials with Flexural yield strength of 89 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 55 °C Show Supplier Material materials with Heat deflection temperature of 55 °C | dry | ISO 75-1/-2 | 2 MPa | ||
165 °C Show Supplier Material materials with Heat deflection temperature of 165 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 95 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 95 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 4.65e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 4.65e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 3.2 [-] Show Supplier Material materials with Dielectric constant of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 27 kV/mm Show Supplier Material materials with Dielectric strength of 27 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 20 [-] Show Supplier Material materials with Dissipation factor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Dissipation factor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1040 g/cm³ Show Supplier Material materials with Density of melt of 1040 g/cm³ | dry | - | ||
Melt volume-flow rate | 250 °C | 22 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 22 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.8 % Show Supplier Material materials with Shrinkage of 1.8 % | dry | ISO 294-4 | Parallel | |
1.8 % Show Supplier Material materials with Shrinkage of 1.8 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2260 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2260 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.109 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.109 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Yellow Card Available |