General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.16 g/cm³ Show Supplier Material materials with Density of 1.16 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | dry | Sim. to ISO 62 |
Water absorption | 7 % Show Supplier Material materials with Water absorption of 7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.06 GPa Show Supplier Material materials with Elastic modulus of 0.06 GPa | dry | ISO 527-1/-2 | |
Elongation | 200 % Show Supplier Material materials with Elongation of 200 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 32 [-] Show Supplier Material materials with Hardness, Shore D of 32 [-] | dry | ISO 868 | 3s |
Tear strength | 80 kN/m Show Supplier Material materials with Tear strength of 80 kN/m | dry | ISO 34-1; Method B | |
Tensile strength | 13.1 MPa Show Supplier Material materials with Tensile strength of 13.1 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Melting point | 212 °C Show Supplier Material materials with Melting point of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.7 [-] Show Supplier Material materials with Dielectric constant of 4.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 310 [-] Show Supplier Material materials with Dissipation factor of 310 [-] | dry | IEC 62631-2-1 | 100Hz |
810 [-] Show Supplier Material materials with Dissipation factor of 810 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 13.5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 13.5 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing membranes, Breathable Outdoor clothing, Medical gowns | |
Certifications | Food Contact |