General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Moisture absorption | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 11 GPa Show Supplier Material materials with Elastic modulus of 11 GPa | conditioned | ISO 527-1/-2 | |
16 GPa Show Supplier Material materials with Elastic modulus of 16 GPa | dry | ISO 527-1/-2 | ||
80 °C | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | dry | ISO 527-1/-2 | |
120 °C | 7 GPa Show Supplier Material materials with Elastic modulus of 7 GPa | dry | ISO 527-1/-2 | |
140 °C | 6.2 GPa Show Supplier Material materials with Elastic modulus of 6.2 GPa | dry | ISO 527-1/-2 | |
160 °C | 5.7 GPa Show Supplier Material materials with Elastic modulus of 5.7 GPa | dry | ISO 527-1/-2 | |
180 °C | 5 GPa Show Supplier Material materials with Elastic modulus of 5 GPa | dry | ISO 527-1/-2 | |
200 °C | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Elongation of 6 % | conditioned | ISO 527-1/-2 | ||
80 °C | 7 % Show Supplier Material materials with Elongation of 7 % | dry | ISO 527-1/-2 | |
120 °C | 8 % Show Supplier Material materials with Elongation of 8 % | dry | ISO 527-1/-2 | |
140 °C | 8.5 % Show Supplier Material materials with Elongation of 8.5 % | dry | ISO 527-1/-2 | |
160 °C | 9.3 % Show Supplier Material materials with Elongation of 9.3 % | dry | ISO 527-1/-2 | |
180 °C | 11 % Show Supplier Material materials with Elongation of 11 % | dry | ISO 527-1/-2 | |
200 °C | 12 % Show Supplier Material materials with Elongation of 12 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 14.0 kJ/m² | dry | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 92 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 92 kJ/m² | dry | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 98 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 98 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | conditioned | ISO 527-1/-2 | |
220 MPa Show Supplier Material materials with Tensile strength of 220 MPa | dry | ISO 527-1/-2 | ||
80 °C | 130 MPa Show Supplier Material materials with Tensile strength of 130 MPa | dry | ISO 527-1/-2 | |
120 °C | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | dry | ISO 527-1/-2 | |
140 °C | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-1/-2 | |
160 °C | 90 MPa Show Supplier Material materials with Tensile strength of 90 MPa | dry | ISO 527-1/-2 | |
180 °C | 85 MPa Show Supplier Material materials with Tensile strength of 85 MPa | dry | ISO 527-1/-2 | |
200 °C | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |