General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.37 g/cm³ Show Supplier Material materials with Density of 1.37 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7.7 GPa Show Supplier Material materials with Elastic modulus of 7.7 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | dry | ISO 527-1/-2 | |
Flexural modulus | 7 GPa Show Supplier Material materials with Flexural modulus of 7 GPa | dry | ISO 178 | |
Flexural yield strength | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 6.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6.5 kJ/m² | dry | ISO 179/1eA |
Tensile strength | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Heat deflection temperature | 276 °C Show Supplier Material materials with Heat deflection temperature of 276 °C | dry | ISO 75-1/-2 | 2 MPa | |
284 °C Show Supplier Material materials with Heat deflection temperature of 284 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 575 V Show Supplier Material materials with Comparative tracking index of 575 V | dry | IEC 60112 | |
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 60250 | 1GHz |
Dielectric strength | 30 kV/mm Show Supplier Material materials with Dielectric strength of 30 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 100 [-] Show Supplier Material materials with Dissipation factor of 100 [-] | dry | IEC 60250 | 1GHz |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | USB-C Connectors | |
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |