General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.17 g/cm³ Show Supplier Material materials with Density of 1.17 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elastic modulus | 7.6 GPa Show Supplier Material materials with Elastic modulus of 7.6 GPa | dry | ISO 527-1/-2 |
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | dry | ISO 527-1/-2 |
Tensile strength | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glass transition temperature | 58.0 °C Show Supplier Material materials with Glass transition temperature of 58.0 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Heat deflection temperature | 153 °C Show Supplier Material materials with Heat deflection temperature of 153 °C | dry | ISO 75-1/-2 | 2 MPa | |
184 °C Show Supplier Material materials with Heat deflection temperature of 184 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 200 °C Show Supplier Material materials with Melting point of 200 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Carbon Fiber |