General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.16 g/cm³ Show Supplier Material materials with Density of 1.16 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Water absorption | 8.5 % Show Supplier Material materials with Water absorption of 8.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 1.5 GPa Show Supplier Material materials with Elastic modulus of 1.5 GPa | conditioned | ISO 527-1/-2 | |
3.6 GPa Show Supplier Material materials with Elastic modulus of 3.6 GPa | dry | ISO 527-1/-2 | ||
Elongation | 10 % Show Supplier Material materials with Elongation of 10 % | dry | ISO 527-1/-2 | |
25 % Show Supplier Material materials with Elongation of 25 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Impact strength, Charpy notched | 23 °C | 4.7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.7 kJ/m² | dry | ISO 179/1eA |
Thermal
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Flammability | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Heat deflection temperature | 85 °C Show Supplier Material materials with Heat deflection temperature of 85 °C | dry | ISO 75-1/-2 | 2 MPa | ||
230 °C Show Supplier Material materials with Heat deflection temperature of 230 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 2 mm | UL746B |
Rheological Properties
Property | Value |
---|
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | MoS2 |