General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.67 g/cm³ Show Supplier Material materials with Density of 1.67 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 10.5 GPa Show Supplier Material materials with Elastic modulus of 10.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 1.7 % Show Supplier Material materials with Elongation of 1.7 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 3.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 250 V Show Supplier Material materials with Comparative tracking index of 250 V | dry | IEC 60112 | |
Dielectric constant | 3.9 [-] Show Supplier Material materials with Dielectric constant of 3.9 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Dielectric constant of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 28.0 kV/mm Show Supplier Material materials with Dielectric strength of 28.0 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 20 [-] Show Supplier Material materials with Dissipation factor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |