General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.47 g/cm³ Show Supplier Material materials with Density of 1.47 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.9 % Show Supplier Material materials with Moisture absorption of 2.9 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7 GPa Show Supplier Material materials with Elastic modulus of 7 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 6 GPa Show Supplier Material materials with Flexural modulus of 6 GPa | dry | ISO 178 | |
Flexural yield strength | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA |
Tensile strength | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 250 °C Show Supplier Material materials with Heat deflection temperature of 250 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.79 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.79 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.79 mm |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 20% Mineral Fiber and PTFE |