General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 41 % Show Supplier Material materials with Bio-based content of 41 % | dry | ASTM D6866-12 Method B |
Density | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 6.4 GPa Show Supplier Material materials with Elastic modulus of 6.4 GPa | conditioned | ISO 527-1/-2 | |
9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | dry | ISO 527-1/-2 | ||
Elongation | 4 % Show Supplier Material materials with Elongation of 4 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongation of 7 % | conditioned | ISO 527-1/-2 | ||
Impact strength, Charpy notched | -30 °C | 8.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 9.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | conditioned | ISO 527-1/-2 | |
165 MPa Show Supplier Material materials with Tensile strength of 165 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |