General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.18 g/cm³ Show Supplier Material materials with Density of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.19 % Show Supplier Material materials with Moisture absorption of 1.19 % | dry | Sim. to ISO 62 | |
Water absorption | 0.88 % Show Supplier Material materials with Water absorption of 0.88 % | dry | ISO 62 | at 23°C after 24h |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.14 GPa Show Supplier Material materials with Elastic modulus of 0.14 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
150 % Show Supplier Material materials with Elongation of 150 % | dry | ISO 527-1/-2 | ||
Hardness, Shore A | 97 [-] Show Supplier Material materials with Hardness, Shore A of 97 [-] | dry | ISO 868 | 3s |
97 [-] Show Supplier Material materials with Hardness, Shore A of 97 [-] | dry | ISO 868 | 15s | |
Hardness, Shore D | 51 [-] Show Supplier Material materials with Hardness, Shore D of 51 [-] | dry | ISO 868 | 3s |
51 [-] Show Supplier Material materials with Hardness, Shore D of 51 [-] | dry | ISO 868 | 15s | |
Tear strength | 123 kN/m Show Supplier Material materials with Tear strength of 123 kN/m | dry | ISO 34-1; Method B | |
Tensile strength | 24 MPa Show Supplier Material materials with Tensile strength of 24 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Glass transition temperature | -78 °C Show Supplier Material materials with Glass transition temperature of -78 °C | dry | ISO 11357-1/-2 | 10°C/min |
Melting point | 204 °C Show Supplier Material materials with Melting point of 204 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat softening temperature | 54 °C Show Supplier Material materials with Vicat softening temperature of 54 °C | dry | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 7 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 7 cm³/10min | dry | ISO 1133 |
Technological properties