Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.04 GPa Show Supplier Material materials with Elastic modulus of 0.04 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 50 % Show Supplier Material materials with Elongation at yield of 50 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 33 [-] Show Supplier Material materials with Hardness, Shore D of 33 [-] | dry | ISO 868 | 15s |
Tensile strength | 20 MPa Show Supplier Material materials with Tensile strength of 20 MPa | dry | ISO 527-1/-2 |
Thermal
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 230 °C | 32 g/10min Show Supplier Material materials with Melt mass-flow rate of 32 g/10min | dry | ISO 1133 | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties