General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.35 g/cm³ Show Supplier Material materials with Density of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Water absorption | 6.3 % Show Supplier Material materials with Water absorption of 6.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 9.3 GPa Show Supplier Material materials with Elastic modulus of 9.3 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 62 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 62 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Thermal diffusivity | 1.12e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.12e-07 mm²/s | dry | - |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 1150 g/cm³ Show Supplier Material materials with Density of melt of 1150 g/cm³ | dry | - |
Specific heat capacity melt | 2110 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |