General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.52 g/cm³ Show Supplier Material materials with Density of 1.52 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Water absorption | 0.5 % Show Supplier Material materials with Water absorption of 0.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 8.5 GPa Show Supplier Material materials with Elastic modulus of 8.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 225 °C Show Supplier Material materials with Heat deflection temperature of 225 °C | dry | ISO 75-1/-2 | 2 MPa | |
245 °C Show Supplier Material materials with Heat deflection temperature of 245 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 255 °C Show Supplier Material materials with Melting point of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |