General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.63 g/cm³ Show Supplier Material materials with Density of 1.63 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 11 GPa Show Supplier Material materials with Elastic modulus of 11 GPa | dry | ISO 527-1/-2 | |
Elongation | 0.6 % Show Supplier Material materials with Elongation of 0.6 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 1.6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 1.6 kJ/m² | dry | ISO 179/1eA |
23 °C | 2 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 10 kJ/m² | dry | ISO 179/1eU |
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 10 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 55.0 MPa Show Supplier Material materials with Tensile strength of 55.0 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Flammability | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
5VA | dry | IEC 60695-11-20 | 1.6 mm | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | |
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | ||
Thermal conductivity | 1 W/(m·K) Show Supplier Material materials with Thermal conductivity of 1 W/(m·K) | dry | ASTM E1461 | through plane | |
5 W/(m·K) Show Supplier Material materials with Thermal conductivity of 5 W/(m·K) | dry | ASTM E1461 | in plane |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 575 V Show Supplier Material materials with Comparative tracking index of 575 V | dry | IEC 60112 | |
Dielectric constant | 3.89 [-] Show Supplier Material materials with Dielectric constant of 3.89 [-] | dry | IEC 60250 | 5GHz |
3.89 [-] Show Supplier Material materials with Dielectric constant of 3.89 [-] | dry | IEC 60250 | 10GHz | |
Dissipation factor | 59 [-] Show Supplier Material materials with Dissipation factor of 59 [-] | dry | IEC 60250 | 10GHz |
60 [-] Show Supplier Material materials with Dissipation factor of 60 [-] | dry | IEC 60250 | 5GHz |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |