General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.21 g/cm³ Show Supplier Material materials with Density of 1.21 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.2 GPa Show Supplier Material materials with Elastic modulus of 0.2 GPa | dry | ISO 527-1/-2 | |
Elongation | 215 % Show Supplier Material materials with Elongation of 215 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 46 [-] Show Supplier Material materials with Hardness, Shore D of 46 [-] | dry | ISO 868 | 3s |
Tensile strength | 21.1 MPa Show Supplier Material materials with Tensile strength of 21.1 MPa | dry | ISO 527-1/-2 |
Thermal
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 10 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 10 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Spider Couplings |