General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.33 g/cm³ Show Supplier Material materials with Density of 1.33 g/cm³ | dry | ISO 1183 |
Water absorption | 1.8 % Show Supplier Material materials with Water absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elongation | 7 % Show Supplier Material materials with Elongation of 7 % | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 250 °C | 14.0 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 14.0 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.4 % Show Supplier Material materials with Shrinkage of 1.4 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |