General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.48 g/cm³ Show Supplier Material materials with Density of 1.48 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 2 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 55.0 MPa Show Supplier Material materials with Tensile strength of 55.0 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 100 °C Show Supplier Material materials with Heat deflection temperature of 100 °C | dry | ISO 75-1/-2 | 2 MPa | |
195 °C Show Supplier Material materials with Heat deflection temperature of 195 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 270 °C | 34 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 34 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.4 % Show Supplier Material materials with Shrinkage of 1.4 % | dry | Sim. to ISO 294-4 | Parallel | |
1.7 % Show Supplier Material materials with Shrinkage of 1.7 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Mineral Powder |