General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 0.69 g/cm³ Show Supplier Material materials with Density of 0.69 g/cm³ | dry | ISO 60 |
1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Water absorption | 0.75 % Show Supplier Material materials with Water absorption of 0.75 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.04 GPa Show Supplier Material materials with Elastic modulus of 0.04 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 77 % Show Supplier Material materials with Elongation at yield of 77 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 33 [-] Show Supplier Material materials with Hardness, Shore D of 33 [-] | dry | ISO 868 | 3s |
Tensile strength | 21 MPa Show Supplier Material materials with Tensile strength of 21 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Glass transition temperature | -78 °C Show Supplier Material materials with Glass transition temperature of -78 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Melting point | 195 °C Show Supplier Material materials with Melting point of 195 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | |
Thermal diffusivity | 6.56e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 6.56e-08 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Dielectric constant of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 10 [-] Show Supplier Material materials with Dissipation factor of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
170 [-] Show Supplier Material materials with Dissipation factor of 170 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 896 g/cm³ Show Supplier Material materials with Density of melt of 896 g/cm³ | dry | - | ||
Melt volume-flow rate | 230 °C | 33 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 33 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1700.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1700.0 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Washing Machine Timer Knobs, Screw Drivers and Plyers, Chair Carriers, Seat Suspension/Fabrics, Soft touch in spatulas and kitchenware, Railway Pads, Conveyor Belts, Arnitel spring in monitor arm, Cosmetic Dispensers, Wine Taps, Grips, Industrial Cords and Ropes, Support Springs, Phone case | |
Certifications | Food Contact, USP class VI, Yellow Card Available |