General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.15 g/cm³ Show Supplier Material materials with Density of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Water absorption | 0.7 % Show Supplier Material materials with Water absorption of 0.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.07 GPa Show Supplier Material materials with Elastic modulus of 0.07 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
950 % Show Supplier Material materials with Elongation of 950 % | dry | ISO 527-1/-2 | ||
Hardness, Shore D | 39 [-] Show Supplier Material materials with Hardness, Shore D of 39 [-] | dry | ISO 868 | 3s |
39 [-] Show Supplier Material materials with Hardness, Shore D of 39 [-] | dry | ISO 868 | 15s | |
Tear strength | 95 kN/m Show Supplier Material materials with Tear strength of 95 kN/m | dry | ISO 34-1; Method B | |
260 kN/m Show Supplier Material materials with Tear strength of 260 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 21.5 MPa Show Supplier Material materials with Tensile strength of 21.5 MPa | dry | ISO 527-1/-2 | |
32 MPa Show Supplier Material materials with Tensile strength of 32 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 213 °C Show Supplier Material materials with Melting point of 213 °C | dry | ISO 11357-1/-3 | 10°C/min |
Thermal diffusivity | 8.6e-08 mm²/s Show Supplier Material materials with Thermal diffusivity of 8.6e-08 mm²/s | dry | - |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1010.0 g/cm³ Show Supplier Material materials with Density of melt of 1010.0 g/cm³ | dry | - | ||
Melt volume-flow rate | 230 °C | 8 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 8 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Shrinkage of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 2220 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2220 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.193 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.193 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Boots and Bellows |