General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.13 g/cm³ Show Supplier Material materials with Density of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.45 % Show Supplier Material materials with Moisture absorption of 0.45 % | dry | Sim. to ISO 62 |
Water absorption | 0.17 % Show Supplier Material materials with Water absorption of 0.17 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.06 GPa Show Supplier Material materials with Elastic modulus of 0.06 GPa | dry | ISO 527-1/-2 | |
Elongation | 350 % Show Supplier Material materials with Elongation of 350 % | dry | ISO 527-1/-2 | |
Hardness, Shore A | 86 [-] Show Supplier Material materials with Hardness, Shore A of 86 [-] | dry | ISO 868 | 3s |
Tensile strength | 8.5 MPa Show Supplier Material materials with Tensile strength of 8.5 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Flammability | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Glass transition temperature | -70 °C Show Supplier Material materials with Glass transition temperature of -70 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Melting point | 172 °C Show Supplier Material materials with Melting point of 172 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dielectric strength | 21 kV/mm Show Supplier Material materials with Dielectric strength of 21 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 1.9e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.9e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 2.7 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 2.7 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |