General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.39 g/cm³ Show Supplier Material materials with Density of 1.39 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.65 % Show Supplier Material materials with Moisture absorption of 1.65 % | dry | Sim. to ISO 62 |
Water absorption | 5.8 % Show Supplier Material materials with Water absorption of 5.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 6.5 GPa Show Supplier Material materials with Elastic modulus of 6.5 GPa | conditioned | ISO 527-1/-2 | |
10.5 GPa Show Supplier Material materials with Elastic modulus of 10.5 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongation of 5 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 9.1 GPa Show Supplier Material materials with Flexural modulus of 9.1 GPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 9.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9.5 kJ/m² | dry | ISO 179/1eA |
Tensile strength | 120 MPa Show Supplier Material materials with Tensile strength of 120 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Tensile strength of 170 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 33% Glass Fiber |