General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.33 g/cm³ Show Supplier Material materials with Density of 1.33 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elongation | 7 % Show Supplier Material materials with Elongation of 7 % | dry | ISO 527-1/-2 |
9 % Show Supplier Material materials with Elongation of 9 % | conditioned | ISO 527-1/-2 | |
Flexural modulus | 4.4 GPa Show Supplier Material materials with Flexural modulus of 4.4 GPa | conditioned | ISO 178 |
7.1 GPa Show Supplier Material materials with Flexural modulus of 7.1 GPa | dry | ISO 178 | |
Flexural yield strength | 125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | conditioned | ISO 178 |
190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
Tensile strength | 88 MPa Show Supplier Material materials with Tensile strength of 88 MPa | conditioned | ISO 527-1/-2 |
135 MPa Show Supplier Material materials with Tensile strength of 135 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 250 °C | 14.0 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 14.0 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |