General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.62 g/cm³ Show Supplier Material materials with Density of 1.62 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Water absorption | 3.9 % Show Supplier Material materials with Water absorption of 3.9 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 17.5 GPa Show Supplier Material materials with Elastic modulus of 17.5 GPa | dry, conditioned | ISO 527-1/-2 | |
Elongation | 2.6 % Show Supplier Material materials with Elongation of 2.6 % | dry, conditioned | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry | ISO 179/1eA |
Tensile strength | 280 MPa Show Supplier Material materials with Tensile strength of 280 MPa | dry, conditioned | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glass transition temperature | 130 °C Show Supplier Material materials with Glass transition temperature of 130 °C | dry | ASTM D5026/D7028 | DMTA (tan d) | |
Heat deflection temperature | 295 °C Show Supplier Material materials with Heat deflection temperature of 295 °C | dry | ISO 75-1/-2 | 2 MPa | |
Melting point | 315 °C Show Supplier Material materials with Melting point of 315 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |