General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.7 g/cm³ Show Supplier Material materials with Density of 1.7 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1 % Show Supplier Material materials with Moisture absorption of 1 % | dry | Sim. to ISO 62 |
Water absorption | 3.6 % Show Supplier Material materials with Water absorption of 3.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | conditioned | ISO 527-1/-2 | |
20 GPa Show Supplier Material materials with Elastic modulus of 20 GPa | dry | ISO 527-1/-2 | ||
Elongation | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongation of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 18.5 GPa Show Supplier Material materials with Flexural modulus of 18.5 GPa | dry | ISO 178 | |
Flexural yield strength | 365 MPa Show Supplier Material materials with Flexural yield strength of 365 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 160 MPa Show Supplier Material materials with Tensile strength of 160 MPa | conditioned | ISO 527-1/-2 | |
240 MPa Show Supplier Material materials with Tensile strength of 240 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 1.64e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.64e-07 mm²/s | dry | - |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1380.0 g/cm³ Show Supplier Material materials with Density of melt of 1380.0 g/cm³ | dry | - | |
Shrinkage | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | dry | ISO 294-4 | Parallel |
0.8 % Show Supplier Material materials with Shrinkage of 0.8 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 1720.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1720.0 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.39 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.39 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 60% Glass Fiber |