General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Water absorption | 0.6 % Show Supplier Material materials with Water absorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.9 GPa Show Supplier Material materials with Elastic modulus of 0.9 GPa | dry | ISO 527-1/-2 | |
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | |
360 % Show Supplier Material materials with Elongation of 360 % | dry | ISO 527-1/-2 | ||
570 % Show Supplier Material materials with Elongation of 570 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.94 GPa Show Supplier Material materials with Flexural modulus of 0.94 GPa | dry | ISO 178 | |
Hardness, Shore D | 71 [-] Show Supplier Material materials with Hardness, Shore D of 71 [-] | dry | ISO 868 | 3s |
Tear strength | 224 kN/m Show Supplier Material materials with Tear strength of 224 kN/m | dry | ISO 34-1; Method B | |
228 kN/m Show Supplier Material materials with Tear strength of 228 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | dry | ISO 527-1/-2 | |
58.0 MPa Show Supplier Material materials with Tensile strength of 58.0 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 4 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 4 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|