General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.37 g/cm³ Show Supplier Material materials with Density of 1.37 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Water absorption | 6.5 % Show Supplier Material materials with Water absorption of 6.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.5 GPa Show Supplier Material materials with Elastic modulus of 3.5 GPa | conditioned | ISO 527-1/-2 | |
7.5 GPa Show Supplier Material materials with Elastic modulus of 7.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 1.9 GPa Show Supplier Material materials with Elastic modulus of 1.9 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.3 % Show Supplier Material materials with Elongation of 2.3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongation of 5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 3.7 % Show Supplier Material materials with Elongation of 3.7 % | dry | ISO 527-1/-2 | |
Flexural modulus | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | conditioned | ISO 178 | |
6.8 GPa Show Supplier Material materials with Flexural modulus of 6.8 GPa | dry | ISO 178 | ||
120 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | dry | ISO 178 | |
160 °C | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | dry | ISO 178 | |
Flexural yield strength | 75 MPa Show Supplier Material materials with Flexural yield strength of 75 MPa | conditioned | ISO 178 | |
145 MPa Show Supplier Material materials with Flexural yield strength of 145 MPa | dry | ISO 178 | ||
120 °C | 45 MPa Show Supplier Material materials with Flexural yield strength of 45 MPa | dry | ISO 178 | |
160 °C | 35 MPa Show Supplier Material materials with Flexural yield strength of 35 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 55.0 MPa Show Supplier Material materials with Tensile strength of 55.0 MPa | conditioned | ISO 527-1/-2 | |
97 MPa Show Supplier Material materials with Tensile strength of 97 MPa | dry | ISO 527-1/-2 | ||
120 °C | 30 MPa Show Supplier Material materials with Tensile strength of 30 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 3.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 180 °C Show Supplier Material materials with Heat deflection temperature of 180 °C | dry | ISO 75-1/-2 | 2 MPa | |
210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Thermal diffusivity | 1.16e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.16e-07 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 500 V Show Supplier Material materials with Comparative tracking index of 500 V | dry | IEC 60112 | |
Dielectric constant | 3.3 [-] Show Supplier Material materials with Dielectric constant of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Dielectric constant of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dissipation factor | 50 [-] Show Supplier Material materials with Dissipation factor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
140 [-] Show Supplier Material materials with Dissipation factor of 140 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Dissipation factor of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3200 [-] Show Supplier Material materials with Dissipation factor of 3200 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1170 g/cm³ Show Supplier Material materials with Density of melt of 1170 g/cm³ | dry | - | ||
Melt mass-flow rate | 25 g/10min Show Supplier Material materials with Melt mass-flow rate of 25 g/10min | dry | ISO 1133 | ||
Melt volume-flow rate | 250 °C | 20 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | dry | ISO 294-4 | Parallel | |
0.93 % Show Supplier Material materials with Shrinkage of 0.93 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2310 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2310 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.32 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.32 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Engine Cover with Air Inlet Filters, Engine Covers, Fans & Shrouds, Exterior Mirror Bases, Cylinder head covers, Instrument panels, Sunroof frame | |
Fillers | 30% Glass Fiber and Mineral Powder |