Novamid® 1015B

Want to keep this datasheet? Save it now in your required format

Description

Novamid® is a high-quality polyamide, that has been developed as a special product line in order to cope with high demand levels from our Japanese customers.
Novamid® has seen various applications in various fields and various regions. From car to packaging, Novamid® is supported by an experienced and wide range of experts.

Datasheet URL:

Novamid® 1015B

This material data has been provided by DSM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.8 %

Show Supplier Material materials with Moisture absorption of 2.8 %

dry

Sim. to ISO 62

Thermal

PropertyValueConditionTesting StandardComment

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt mass-flow rate

230 °C

24 g/10min

Show Supplier Material materials with Melt mass-flow rate of 24 g/10min

dry

ISO 1133

Melt volume-flow rate

230 °C

21 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 21 cm³/10min

dry

ISO 1133

Viscosity number

150 cm³/gr

Show Supplier Material materials with Viscosity number of 150 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties