General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.21 g/cm³ Show Supplier Material materials with Density of 1.21 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.12 GPa Show Supplier Material materials with Elastic modulus of 0.12 GPa | dry | ISO 527-1/-2 | |
Elongation | 205 % Show Supplier Material materials with Elongation of 205 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 45 [-] Show Supplier Material materials with Hardness, Shore D of 45 [-] | dry | ISO 868 | 3s |
Tensile strength | 19.5 MPa Show Supplier Material materials with Tensile strength of 19.5 MPa | dry | ISO 527-1/-2 |
Thermal
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 9.6 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9.6 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|