General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Bio-based content | 43 % Show Supplier Material materials with Bio-based content of 43 % | dry | ASTM D6866-12 Method B | |
Density | 1.14 g/cm³ Show Supplier Material materials with Density of 1.14 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | dry | Sim. to ISO 62 | |
Water absorption | 0.14 % Show Supplier Material materials with Water absorption of 0.14 % | dry | ISO 62 | at 23°C after 24h |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.09 GPa Show Supplier Material materials with Elastic modulus of 0.09 GPa | dry | ISO 527-1/-2 | |
Elongation | 250 % Show Supplier Material materials with Elongation of 250 % | dry | ISO 527-1/-2 | |
700 % Show Supplier Material materials with Elongation of 700 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | dry | ISO 178 | |
Hardness, Shore D | 45 [-] Show Supplier Material materials with Hardness, Shore D of 45 [-] | dry | ISO 868 | 3s |
Tear strength | 106 kN/m Show Supplier Material materials with Tear strength of 106 kN/m | dry | ISO 34-1; Method B | |
107 kN/m Show Supplier Material materials with Tear strength of 107 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 17 MPa Show Supplier Material materials with Tensile strength of 17 MPa | dry | ISO 527-1/-2 | |
24 MPa Show Supplier Material materials with Tensile strength of 24 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 39 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 39 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | Sim. to ISO 294-4 | Parallel | ||
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | ISO 294-4 | Normal | ||
1.5 % Show Supplier Material materials with Shrinkage of 1.5 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Smokable Sausage Casings, Phone case | |