Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 4 GPa Show Supplier Material materials with Flexural modulus of 4 GPa | dry | ISO 178 | |
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | dry | ISO 178 | |
Impact strength, Charpy unnotched | 23 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 5 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 189 °C Show Supplier Material materials with Heat deflection temperature of 189 °C | dry | ISO 75-1/-2 | 2 MPa | |
215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 250 °C | 52 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 52 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Glass Fiber |