General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Water absorption | 5.9 % Show Supplier Material materials with Water absorption of 5.9 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 7 GPa Show Supplier Material materials with Elastic modulus of 7 GPa | conditioned | ISO 527-1/-2 | |
11.5 GPa Show Supplier Material materials with Elastic modulus of 11.5 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongation of 7 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 9.7 GPa Show Supplier Material materials with Flexural modulus of 9.7 GPa | dry | ISO 178 | |
Flexural yield strength | 255 MPa Show Supplier Material materials with Flexural yield strength of 255 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 24 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | conditioned | ISO 527-1/-2 | |
195 MPa Show Supplier Material materials with Tensile strength of 195 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Thermal diffusivity | 1.1e-07 mm²/s Show Supplier Material materials with Thermal diffusivity of 1.1e-07 mm²/s | dry | - |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 500 V Show Supplier Material materials with Comparative tracking index of 500 V | conditioned | IEC 60112 | |
Dielectric constant | 3.3 [-] Show Supplier Material materials with Dielectric constant of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Dielectric strength of 35 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 50 [-] Show Supplier Material materials with Dissipation factor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Dissipation factor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1100 [-] Show Supplier Material materials with Dissipation factor of 1100 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Dissipation factor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1150 g/cm³ Show Supplier Material materials with Density of melt of 1150 g/cm³ | dry | - | ||
Melt mass-flow rate | 275 °C | 48 g/10min Show Supplier Material materials with Melt mass-flow rate of 48 g/10min | dry | ISO 1133 | |
Melt volume-flow rate | 275 °C | 40 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 40 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | dry | ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Shrinkage of 1 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2110 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 35% Glass Fiber |