General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.62 g/cm³ Show Supplier Material materials with Density of 1.62 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 12.5 GPa Show Supplier Material materials with Elastic modulus of 12.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 11.5 GPa Show Supplier Material materials with Flexural modulus of 11.5 GPa | dry | ISO 178 | |
Flexural yield strength | 285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 200 MPa Show Supplier Material materials with Tensile strength of 200 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5.3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.3e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 270 °C Show Supplier Material materials with Heat deflection temperature of 270 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 3 mm |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Comparative tracking index | 200 V Show Supplier Material materials with Comparative tracking index of 200 V | dry | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 33% Glass Fiber |