General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Water absorption | 0.65 % Show Supplier Material materials with Water absorption of 0.65 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 0.17 GPa Show Supplier Material materials with Elastic modulus of 0.17 GPa | dry | ISO 527-1/-2 | ||
Elongation | 300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
420 % Show Supplier Material materials with Elongation of 420 % | dry | ISO 527-1/-2 | |||
820 % Show Supplier Material materials with Elongation of 820 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.2 GPa Show Supplier Material materials with Flexural modulus of 0.2 GPa | dry | ISO 178 | ||
Hardness, Shore D | 52 [-] Show Supplier Material materials with Hardness, Shore D of 52 [-] | dry | ISO 868 | 3s | |
Impact strength, Charpy notched | -30 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m² | dry | ISO 179/1eA | |
Tear strength | 132 kN/m Show Supplier Material materials with Tear strength of 132 kN/m | dry | ISO 34-1; Method B | ||
142 kN/m Show Supplier Material materials with Tear strength of 142 kN/m | dry | ISO 34-1; Method B | |||
Tensile strength | 46 MPa Show Supplier Material materials with Tensile strength of 46 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Melting point | 207 °C Show Supplier Material materials with Melting point of 207 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | |
Vicat softening temperature | 90 °C Show Supplier Material materials with Vicat softening temperature of 90 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 21 kV/mm Show Supplier Material materials with Dielectric strength of 21 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 400 [-] Show Supplier Material materials with Dissipation factor of 400 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 9 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Mandrels as Supportive Tool, Hydraulic Hoses, Vacuum Bags | |
Certifications | Yellow Card Available |