General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.81 g/cm³ Show Supplier Material materials with Density of 1.81 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 18.5 GPa Show Supplier Material materials with Elastic modulus of 18.5 GPa | dry | ISO 527-1/-2 | |
Elongation | 1.7 % Show Supplier Material materials with Elongation of 1.7 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 8.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 8.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8.5 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 205 MPa Show Supplier Material materials with Tensile strength of 205 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
4.8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.8e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 232 °C Show Supplier Material materials with Heat deflection temperature of 232 °C | dry | ISO 75-1/-2 | 2 MPa | |
250 °C Show Supplier Material materials with Heat deflection temperature of 250 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 255 °C Show Supplier Material materials with Melting point of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 3.5 [-] Show Supplier Material materials with Dielectric constant of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielectric constant of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dissipation factor | 20 [-] Show Supplier Material materials with Dissipation factor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
110 [-] Show Supplier Material materials with Dissipation factor of 110 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |