General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.18 g/cm³ Show Supplier Material materials with Density of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3 % Show Supplier Material materials with Moisture absorption of 3 % | dry | Sim. to ISO 62 | |
Water absorption | 3.1 % Show Supplier Material materials with Water absorption of 3.1 % | dry | ISO 62 | at 23°C after 24h |
11.5 % Show Supplier Material materials with Water absorption of 11.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 3.7 GPa Show Supplier Material materials with Elastic modulus of 3.7 GPa | dry | ISO 527-1/-2 | |
120 °C | 1.4 GPa Show Supplier Material materials with Elastic modulus of 1.4 GPa | dry | ISO 527-1/-2 | |
Elongation | 10 % Show Supplier Material materials with Elongation of 10 % | dry | ISO 527-1/-2 | |
120 °C | 24 % Show Supplier Material materials with Elongation of 24 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | -30 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
Tensile strength | 95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 | |
120 °C | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | dry | ISO 527-1/-2 |
Thermal
Technological properties
Property | ||
---|---|---|
Fillers | 8% Glass Fiber |