Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.67 g/cm³ Show Supplier Material materials with Density of 1.67 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Water absorption | 0.45 % Show Supplier Material materials with Water absorption of 0.45 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | dry | ISO 527-1/-2 | |
Elongation | 1.5 % Show Supplier Material materials with Elongation of 1.5 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 235 °C Show Supplier Material materials with Heat deflection temperature of 235 °C | dry | ISO 75-1/-2 | 2 MPa | |
250 °C Show Supplier Material materials with Heat deflection temperature of 250 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 255 °C Show Supplier Material materials with Melting point of 255 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Thermal conductivity | 0.65 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.65 W/(m·K) | dry | ASTM E1461 | through plane | |
1.6 W/(m·K) Show Supplier Material materials with Thermal conductivity of 1.6 W/(m·K) | dry | ASTM E1461 | in plane |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielectric constant | 14.0 [-] Show Supplier Material materials with Dielectric constant of 14.0 [-] | dry | IEC 60250 | 1 |
Dielectric strength | 1.1 kV/mm Show Supplier Material materials with Dielectric strength of 1.1 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 3e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 3e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Foglamps, LED Headlight Lighting Modules and Lensholders, Lens holder Sun load, Bezel (Black) Sun load, LED module frame | |
Fillers | 35% Glass Fiber |