General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.16 g/cm³ Show Supplier Material materials with Density of 1.16 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | dry | Sim. to ISO 62 |
Water absorption | 7 % Show Supplier Material materials with Water absorption of 7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.05 GPa Show Supplier Material materials with Elastic modulus of 0.05 GPa | dry | ISO 527-1/-2 | |
Elongation | 450 % Show Supplier Material materials with Elongation of 450 % | dry | ISO 527-1/-2 | |
810 % Show Supplier Material materials with Elongation of 810 % | dry | ISO 527-1/-2 | ||
Flexural modulus | 0.04 GPa Show Supplier Material materials with Flexural modulus of 0.04 GPa | dry | ISO 178 | |
Hardness, Shore D | 32 [-] Show Supplier Material materials with Hardness, Shore D of 32 [-] | dry | ISO 868 | 3s |
Tear strength | 93 kN/m Show Supplier Material materials with Tear strength of 93 kN/m | dry | ISO 34-1; Method B | |
95 kN/m Show Supplier Material materials with Tear strength of 95 kN/m | dry | ISO 34-1; Method B | ||
Tensile strength | 14.0 MPa Show Supplier Material materials with Tensile strength of 14.0 MPa | dry | ISO 527-1/-2 | |
18 MPa Show Supplier Material materials with Tensile strength of 18 MPa | dry | ISO 527-1/-2 | Normal |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
1.5e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Melting point | 212 °C Show Supplier Material materials with Melting point of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat softening temperature | 124 °C Show Supplier Material materials with Vicat softening temperature of 124 °C | dry | ISO 306 | 50°C/h 10N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | |
Dielectric constant | 4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.7 [-] Show Supplier Material materials with Dielectric constant of 4.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 20 kV/mm Show Supplier Material materials with Dielectric strength of 20 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 310 [-] Show Supplier Material materials with Dissipation factor of 310 [-] | dry | IEC 62631-2-1 | 100Hz |
810 [-] Show Supplier Material materials with Dissipation factor of 810 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 32 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 32 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.55 % Show Supplier Material materials with Shrinkage of 1.55 % | dry | ISO 294-4 | Parallel | |
1.75 % Show Supplier Material materials with Shrinkage of 1.75 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Body Plugs |