General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.04 GPa Show Supplier Material materials with Elastic modulus of 0.04 GPa | dry | ISO 527-1/-2 | |
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | ||
Hardness, Shore D | 30 [-] Show Supplier Material materials with Hardness, Shore D of 30 [-] | dry | ISO 868 | 3s |
Tensile strength | 19 MPa Show Supplier Material materials with Tensile strength of 19 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Melting point | 195 °C Show Supplier Material materials with Melting point of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt volume-flow rate | 230 °C | 34 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 34 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |