General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 0.95 g/cm³ Show Supplier Material materials with Density of 0.95 g/cm³ | dry | ISO 1183 |
Water absorption | 0.8 % Show Supplier Material materials with Water absorption of 0.8 % | dry | Sim. to ISO 62 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.02 GPa Show Supplier Material materials with Elastic modulus of 0.02 GPa | dry | ISO 527-1/-2 | |
Elongation | 650 % Show Supplier Material materials with Elongation of 650 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 25 [-] Show Supplier Material materials with Hardness, Shore D of 25 [-] | dry | ISO 868 | 3s |
Tensile strength | 9 MPa Show Supplier Material materials with Tensile strength of 9 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
2.2e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Glass transition temperature | -74 °C Show Supplier Material materials with Glass transition temperature of -74 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
-45 °C Show Supplier Material materials with Glass transition temperature of -45 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Melting point | 195 °C Show Supplier Material materials with Melting point of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 905 g/cm³ Show Supplier Material materials with Density of melt of 905 g/cm³ | dry | - | |
Melt volume-flow rate | 190 °C | 5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 5 cm³/10min | dry | ISO 1133 |
Technological properties