General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 26 GPa Show Supplier Material materials with Elastic modulus of 26 GPa | dry | ISO 527-1/-2 | |
150 °C | 11.8 GPa Show Supplier Material materials with Elastic modulus of 11.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 1.3 % Show Supplier Material materials with Elongation of 1.3 % | dry | ISO 527-1/-2 | |
150 °C | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
Impact strength, Charpy notched | 23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA |
Impact strength, Charpy unnotched | 23 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU |
Tensile strength | 280 MPa Show Supplier Material materials with Tensile strength of 280 MPa | dry | ISO 527-1/-2 | |
150 °C | 117 MPa Show Supplier Material materials with Tensile strength of 117 MPa | dry | ISO 527-1/-2 |
Thermal
Technological properties
Property | ||
---|---|---|
Fillers | 30% Carbon Fiber |