General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.26 g/cm³ Show Supplier Material materials with Density of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Water absorption | 0.6 % Show Supplier Material materials with Water absorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 0.25 GPa Show Supplier Material materials with Elastic modulus of 0.25 GPa | dry | ISO 527-1/-2 | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 23 % Show Supplier Material materials with Elongation at yield of 23 % | dry | ISO 527-1/-2 | ||
Hardness, Shore D | 55.0 [-] Show Supplier Material materials with Hardness, Shore D of 55.0 [-] | dry | ISO 868 | 15s | |
Impact strength, Charpy notched | -30 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 6 kJ/m² | dry | ISO 179/1eU | |
Tear strength | 165 kN/m Show Supplier Material materials with Tear strength of 165 kN/m | dry | ISO 34-1; Method B |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1.6e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 80 °C Show Supplier Material materials with Heat deflection temperature of 80 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 195 °C Show Supplier Material materials with Melting point of 195 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | dry | UL746B | 0.75 mm | ||
Vicat softening temperature | 85 °C Show Supplier Material materials with Vicat softening temperature of 85 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard |
---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt mass-flow rate | 230 °C | 9.5 g/10min Show Supplier Material materials with Melt mass-flow rate of 9.5 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Convoluted Tubes | |
Certifications | Yellow Card Available |