General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.48 g/cm³ Show Supplier Material materials with Density of 1.48 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongation | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 4.2 GPa Show Supplier Material materials with Flexural modulus of 4.2 GPa | conditioned | ISO 178 | |
6 GPa Show Supplier Material materials with Flexural modulus of 6 GPa | dry | ISO 178 | ||
Flexural yield strength | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | conditioned | ISO 178 | |
175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 6.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m² | conditioned | ISO 179/1eA | |
Tensile strength | 118 MPa Show Supplier Material materials with Tensile strength of 118 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 25 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 25 cm³/10min | dry | ISO 1133 | |
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Shrinkage of 1.1 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |