General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.18 g/cm³ Show Supplier Material materials with Density of 1.18 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Water absorption | 7.6 % Show Supplier Material materials with Water absorption of 7.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 10 % Show Supplier Material materials with Elongation of 10 % | dry | ISO 527-1/-2 | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural modulus | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | dry | ISO 178 | |
Flexural yield strength | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | 23 °C | 4.7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 4.7 kJ/m² | dry | ISO 179/1eA |
Thermal
Technological properties
Property |
---|