General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Water absorption | 5.7 % Show Supplier Material materials with Water absorption of 5.7 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 4.5 GPa Show Supplier Material materials with Elastic modulus of 4.5 GPa | conditioned | ISO 527-1/-2 | |
9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | dry | ISO 527-1/-2 | ||
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-1/-2 | |
8 % Show Supplier Material materials with Elongation of 8 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 7.5 GPa Show Supplier Material materials with Flexural modulus of 7.5 GPa | dry | ISO 178 | |
Flexural yield strength | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | dry | ISO 179/1eA | |
23 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 35 kJ/m² | dry | ISO 179/1eA | |
23 °C | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 40 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 95 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 115 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 115 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 105 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 105 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | conditioned | ISO 527-1/-2 | |
125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Snowmobile Front- and Rear Bumbers, Snowmobile Rear Seat Handle, Lawnmower Steering Tower | |
Fillers | 33% Glass Fiber |